Customization: | Available |
---|---|
Molecular Principal Chain: | Heterochain Polymer |
Color: | Any Colors Can Be Customized |
Still deciding? Get samples of US$ 1.5/kg
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Product Description: |
Advantage: |
Application |
Item No | Description | Application | ||||||||
RY-E50180VC | 80ºC insulation grade PVC Compounds for automotive thin- wall wires | Comply with JIS C3406, JASO D611-94,SAEJ1128 and similar standards | ||||||||
RY-E50290VC | 90ºC Environmentally friendly insulation grade PVC Compounds for automotive wires | Apply for the thin-wall and low-voltage cable insulation, Comply with JASO D611standards. Small size wire can meet the ISO 6722 scratch resistance test | ||||||||
RY-E503105VC | 105ºC insulation grade PVC Compounds for automotive thin -wall wires | Comply with DIN72551,VW60306-2005,LV112 and similar standards | ||||||||
RY-E504105VC | 105ºC Environmentally friendly insulation grade PVC Compounds for automotive wires | Comply with German standard 105ºC grade, Franch standard T2 grade or National industry standard QVR-105 grade. meet the heat resistance requirements for thin-wall automotive wire insulation. | ||||||||
RY-E505105VC | 105ºC Environmentally friendly insulation grade soft PVC Compounds for automotive wires | Apply for 105ºC grade automobile battery wire |
Technical Properities: |
No | Item | Unit | RY-E50180VC | RY-E50290VC | RY-E503105VC | RY-E504105VC | RY-E505105VC |
1 | Tensile Strength | MPa | ≥18 | ≥16 | ≥18 | ≥16 | ≥16 |
2 | Elongation at Break | % | ≥200 | ≥150 | ≥250 | ≥150 | ≥180 |
3 | Thermal Deformation | % | ≤30 | ≤40 | ≤30 | --- | ≤30 |
4 | Impact Brittleness Temperature | ºC | -20 | -20 | -25 | -20 | -25 |
5 | Thermal stability time at 200ºC | min | ≥120 | ≥80 | ≥200 | ≥80 | ≥80 |
6 | Volume Resistivity at 20ºC | Ω.m | ≥1.0×1011 | ≥1.0×1011 | ≥1.0×1012 | ≥1.0×1011 | ≥1.0×1011 |
7 | Work Temperature | ºC | 80 | --- | 95±1 | --- | --- |
Volume Resistivity at Work Temperature | Ω.m | ≥1.0×108 | --- | ≥1.0×108 | --- | --- | |
8 | Dielectric Strength | MV/m | --- | ≥20 | --- | ≥20 | --- |
9 | Thermal Aging Performance(IEC) | ºC× day | 121×7 | 120×7 | 136×7 | 135×7 | 135×7 |
Tensile Strength after Aging | MPa | --- | ≥16 | --- | ≥16 | ≥16 | |
Retention Rate of Tensile Strength after Aging | % | ≥85 | ≥75 | ≥80 | ≥75 | ≥75 | |
Elongation at Break after Aging | % | --- | ≥150 | --- | ≥150 | ≥150 | |
Retention Rate of Elongation at Break after Aging | % | ≥65 | ≥75 | ≥80 | ≥75 | ≥75 | |
10 | Thermal Aging Performance(IEC) | ºCx day | --- | --- | --- | 125×10 | --- |
Tensile Strength after Aging | MPa | --- | --- | --- | ≥16 | --- | |
Elongation at Break after Aging | % | --- | --- | --- | ≥150 | --- | |
Mass Loss | mg/cm2 | --- | --- | --- | 2 | --- | |
11 | Oil Resistant Test(IRM902oil,50ºCx24h) | ||||||
Change Rate of Tensile Strength | % | --- | ≤±25 | --- | ≤±25 | ≤±25 | |
Change Rate of Elongation at Break | % | --- | ≤±25 | --- | ≤±25 | ≤±25 | |
12 | Hardness | ShoreA | 92±3 | --- | 92±3 | --- | --- |